Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of RADILON A RV350W 333 BK - PA66-GF35 - RadiciGroup High Performance Polymers

Material Data Center offers the following functions for RADILON A RV350W 333 BK:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Radilon A datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts
PA66 35% glass fibre reinforced injection moulding grade. Heat stabilized. Black colour.


Suitable for parts requiring high stiffness, good mechanical resistance and excellent heat ageing properties retention.

Processing/Physical Characteristicsdry / condUnitTest Standard
ISO Data
Molding shrinkage, parallel 0.3 / * % ISO 294-4, 2577
Molding shrinkage, normal 1.0 / * % ISO 294-4, 2577
Mechanical propertiesdry / condUnitTest Standard
ISO Data
Tensile Modulus 10800 / 8000 MPa ISO 527
Stress at break 185 / 125 MPa ISO 527
Strain at break 3.1 / 5 % ISO 527
Charpy impact strength, +23°C 85 / 95 kJ/m² ISO 179/1eU
Charpy impact strength, -30°C 70 / - kJ/m² ISO 179/1eU
Charpy notched impact strength, +23°C 12 / 19 kJ/m² ISO 179/1eA
Charpy notched impact strength, -30°C 11 / - kJ/m² ISO 179/1eA
Thermal propertiesdry / condUnitTest Standard
ISO Data
Melting temperature, 10°C/min 260 / * °C ISO 11357-1/-3
Temp. of deflection under load, 1.80 MPa 250 / * °C ISO 75-1/-2
Temp. of deflection under load, 0.45 MPa 255 / * °C ISO 75-1/-2
Vicat softening temperature, B 250 / * °C ISO 306
Coeff. of linear therm. expansion, parallel 24 / * E-6/K ISO 11359-1/-2
Coeff. of linear therm. expansion, normal 97 / * E-6/K ISO 11359-1/-2
Burning Behav. at thickness h HB / * class IEC 60695-11-10
Thickness tested 0.8 / * mm -
Electrical propertiesdry / condUnitTest Standard
ISO Data
Volume resistivity 1E13 / 1E11 Ohm*m IEC 62631-3-1
Surface resistivity * / 1E10 Ohm IEC 62631-3-2
Other propertiesdry / condUnitTest Standard
Water absorption 5.5 / * % Sim. to ISO 62
Humidity absorption 1.5 / * % Sim. to ISO 62
Density 1400 / - kg/m³ ISO 1183
Processing Recommendation Injection MoldingValueUnitTest Standard
Pre-drying - Temperature 80 °C -
Pre-drying - Time 2 - 4 h -
Processing humidity ≤0.15 % -
Melt temperature 280 - 300 °C -
Mold temperature 80 - 100 °C -
Diagrams
Viscosity-shear rate , RADILON A RV350W 333 BK, PA66-GF35, RadiciGroup
Shearstress-shear rate , RADILON A RV350W 333 BK, PA66-GF35, RadiciGroup
Stress-strain , RADILON A RV350W 333 BK (dry), PA66-GF35, RadiciGroup
Stress-strain , RADILON A RV350W 333 BK (cond.), PA66-GF35, RadiciGroup
Secant modulus-strain , RADILON A RV350W 333 BK (dry), PA66-GF35, RadiciGroup
Secant modulus-strain , RADILON A RV350W 333 BK (cond.), PA66-GF35, RadiciGroup
Specific volume-temperature (pvT) , RADILON A RV350W 333 BK, PA66-GF35, RadiciGroup
Tensile modulus-temperature , RADILON A RV350W 333 BK (dry), PA66-GF35, RadiciGroup
Tensile modulus-temperature , RADILON A RV350W 333 BK (cond.), PA66-GF35, RadiciGroup
LTHA-Stress at Break 4mm, RADILON A RV350W 333 BK, PA66-GF35, RadiciGroup
LTHA-Strain at Break 4mm, RADILON A RV350W 333 BK, PA66-GF35, RadiciGroup
LTHA-Charpy Notched Impact Strength (23°C) 4mm, RADILON A RV350W 333 BK, PA66-GF35, RadiciGroup
Characteristics
Processing
Injection Molding
Delivery form
Granules, Black
Additives
Release agent
Special Characteristics
Heat stabilized or stable to heat
Regional Availability
Other text information
Injection molding
The material is delivered in moisture-proof packaging ready for processing. Maximum recommended water content for best processing is 0.15%. Typical conditions with a desiccant drier: temperature 80 ° C, dew point -20 ° C or below, time 2-4 h or more. Special care must be taken to avoid moisture absorption and contamination with other polymers when adding regrind material. Colour variation and mechanical properties reduction may occur and should always be carefully monitored.

Injection Molding Processing Parameters
Melt TemperatureMold TemperatureInjection Speed
280 - 300°C80 - 100°Cmedium-high
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com